Phase |
Ingredient |
% Wt. |
INCI Name
|
A |
Water |
q.s |
|
|
Carbopol 980 |
0.3 |
Carbomer |
|
Hydro Wrap Black IO |
10.0 |
Black Iron Oxide
/Dimethicone
Copolyol
|
|
Hydrophilic Kaolin |
3.0 |
Kaolin/Dimethicone
Copolyol
|
|
|
|
|
B |
PEG-20 Beeswax |
2.0 |
PEG-20 Beeswax |
|
Carnauba Wax |
6.0 |
Carnauba Wax |
|
Beeswax |
3.0 |
Beeswax |
|
Candelilla |
6.0 |
Candelilla |
|
Stearic Acid XXX |
2.0 |
Stearic Acid |
|
|
|
|
C |
Water |
2.0 |
|
|
Triethanolamine |
1.3 |
Triethanolamine |
|
|
|
|
D |
Syntran 520 |
7.0 |
Acrylate
Copolyer/Propylene Glycol/Sodium Laureth-12 Sulfate
|
|
Aquamere S-2012 |
3.0 |
PVP/Dimethiconylacrylate/
Polycarbamyl/Polyglycol
Ester
|
|
|
|
|
E |
Germaben II-E |
1.0 |
Propylene Glycol/Diazolidinyl
Urea/Methylparaben/
Propylparaben
|
Procedure:
In the final mixing kettle,
charge with water and disperse in the Carbopol; mix for 15 minutes.
Add remaining Phase A ingredients in order listed; begin heating to 80°C.
In a separate container, weigh out Phase B ingredients, and begin
heating to 82°C.
When both Phases are at the proper temperature, combine Phase B into
Phase A and mix for
5 minutes. Now add
pre-mixed Phase C to combined Phase A and B with side-sweep and
homogenizer mixing, and mix for 5 minutes. Begin cooling Phase A and B
with
side-sweep and homogenizer
mixing, and mix for 5 minutes. Begin cooling batch with side-sweep
agitation dawn to 40°C.
At 40°C
add Phase D ingredients in order listed and resume cooling. At 30°C
add Phase E and mix for 5 minutes. Batch is complete.
If you don't find what you're looking for,
Contact Us.
We may have a suitable product that's not listed, or we may be
able to develop a material to fit your specific needs.
Tel : (02)2217-3442 / Fax : (02)2704-4070
|